Superalloy is a kind of metal that works for a long time under the action of high temperature above 600℃ and certain and certain stress. The characteristics of superalloys that are different from traditional metals and alloys are: the alloys have high strength under high temperature working environment, good oxidation resistance and hot corrosion resistance, good fatigue properties, fracture toughness, and maintain good performance at various temperatures. comprehensive performance such as organizational stability and operational reliability.

Superalloys can be divided into iron-based superalloys, nickel-based superalloys and cobalt-based superalloys according to the types of matrix elements. Among them, nickel-based superalloys have relatively stronger heat resistance, so they are the most widely used and are widely used in today's production. The proportion is as high as 80%; according to the manufacturing process, it can be divided into deformed superalloy, cast superalloy and powder superalloy.

We provide you with a variety of product forms, including but not limited to:
• Bar/Rod • Pipe/Tube • Coil/Strip • Plate/Sheet/Circle • Wire • Fitting (Flange, Elbow, Tee...) • Customize

Email: [email protected]
WhatsApp: 0086-13788924073

Chat Online     Leave Message

● Any type and size can be custom made.

● Minimum order quantity: from 10 kg

● Payment method: FOB Shanghai etc., CNY or USD

● Shipping method: sea, railway, air transport

● Packing: strong packaging

ASTM UNS W-Nr. JIS KS Element DIN EN/DIN
Incoloy800 N08800 1.4876 NCF800/2B NCF800 GH20 0Cr20Ni32AlTi X10NiCrAlTi32-20
Incoloy800H N08810 1.4958 NCF800H 1Cr20Ni32AlTi X10NiCrAlTi32-20
Incoloy800HT N08811 1.4959 0Cr25Ni35AlTi
Incoloy825 N08825 2.4858 NCF825 NCF825 0Cr21Ni42Mo3Cu2Ti NiCr21Mo
Incoloy901
Incoloy925 N09925
Incoloy926 N08926 1.4529
Inconel600 N06600 2.4816 NCF1B NCF600 GH600 1Cr15Ni75Fe8 NiCr15Fe8
Inconel601 N06601 2.4851 NCF601 NCF601 1Cr23Ni60Fe13Al NiCr23Fe
Inconel625 N06625 2.4856 NCF625 NCF625 0Cr20Ni65Mo10Nb4 NiCr22Mo9Nb
Inconel690 N06690 2.4642 0Cr30Ni60Fe10 NiCr29Fe
Inconel718 N07718 2.4668 GH169 NiCr19Fe19Nb5Mo3
Inconel725 N07725
Inconel X-750 N07750 2.4669 NCF750 GH145 XCr15Fe7TiAl
HC-276 N10276 2.4819 00Cr15Ni60Mo16W5Fe5 NiMo15Cr15W
HB N10001 2.4800* 0Ni65Mo28Fe5V S-NiMo 30
HB-2 N10665 3.4617 00Ni70Mo28 NiMo28
HB-3 N10675 2.4600* NiMo29Cr
HC N10002 2.4819 0Cr15Ni60Mo16W5Fe5 NiMo16Cr15W
HC-4 N06455 2.4610* 00Cr16Ni65Mo16Ti NiMo16Cr16Ti
HC-22 N06022 2.4602 NiMo21Cr14W
HC-2000 N06200 2.4675 NiCr23Mo16Cu
Hastelloy-X N06002 2.4465
Monel400 N04400 2.4360,2.4361
MonelK500 N05500 2.4375
Monel401 N04401
Monel404 2.4867
Ni 200 N02200 2.4066
Ni 201 N02201
Nitronic50 S20910 XM-19
Nitronic60 S21800 Alloy218
Alloy20 Cb-3 N08020 2.4660* Carpeter20Cb-3 0Cr20Ni35Mo3Cu4Nb NiCr20CuMo
Alloy31 N08031 1.4562 X1NiCrMoCu 32-28-7
Alloy33 N08033 1.4591 X1NiCrMoCuN 33-32-1
ASTM UNS W-Nr. JIS KS Element DIN EN/DIN
Alloy20 Cb-3 N08020 2.4660* Carpeter20Cb-3 0Cr20Ni35Mo3Cu4Nb NiCr20CuMo
IncoloyA-286 S66286 1.4980,1.4944 SUH660
Incoloy800 NO8800 1.4876 NCF800B NCF2B GH20 0Cr20Ni32AlTi X2NiCrAlTi3220
Nimonic75 2.4951
N06219 2.4855 NiCr19Mo9Si
HastelloyX N06002 2.4613
Inconel600 N06600 2.4816 NCF1B NCF600 GH600 1Cr15Ni75Fe8 NiCr15Fe8
Inconel625 N06625 2.4856 NCF625 NCF625 NS3306 0Cr20Ni65Mo10Nb4 NiCr22Mo9Nb
InconelX-750 N07750 2.4669 NCF750 XCr15Fe7TiAl
Nimonic80A N07080 2.4952
Inconel718 N07718 2.4668 GH4169
Inconel725 N07725
Incoloy925 N09925
Inconel600 N06600 2.4816 NCF600 NCF1B 1Cr15Ni75Fe8 LC-NiCr15Fe
PB
Alloy4
Alloy31 N08031 1.4562
F15
Invar36 K93600 1.3912
Material Monel/Inconel/Hastelloy/Duplex Steel/PH Steel/Nickel Alloy
Shape Round,Forging,Ring,Coil,Flange,Disc,Foil,Spherical,Ribbon,Square,Bar,Pipe,Sheet
Grade Duplex:2205(UNS S31803/S32205),2507(UNS S32750),UNS S32760(Zeron 100),2304,904L
Others:253Ma,254SMo,654SMo,F50(UNSS32100)F60,F61,F65,1J22,N4,N6 etc
Alloy: Alloy 20/28/31
Hastelloy:HastelloyB/ -2/B-3/C22/C-4/S/C276/C-2000/G-35/G-30/X/N/g
Hastelloy B/UNS N10001, Hastelloy B-2/UNS N10665/DIN W. Nr. 2.4617, Hastelloy C,
Hastelloy C-4/UNS N06455/DIN W. Nr. 2.4610, Hastelloy C22/UNS N06022/DIN W. Nr. 2.4602,
Hastelloy C276/UNS N10276/DIN W. Nr. 2.4819, Hastelloy X/UNS N06002/DIN W. Nr. 2.4665
Haynes: Haynes 230/556/188
Inconel 600/601/602CA/617/625/713/718/738/X-750,Carpenter 20
Inconel 718 / UNS N07718 / DIN W. Nr. 2.4668,Inconel 601 / UNS N06601 / DIN W. Nr. 2.4851,
Inconel 625 / UNS N06625 / DIN W. Nr. 2.4856,Inconel 725 / UNS N07725,Inconel X-750 / UNS N07750 / DIN W. Nr. 2.4669,Inconel 600 / UNS N06600 / DIN W. Nr. 2.4816
Incoloy: Incoloy 800/800H/800HT/825/925/926;
GH: GH2132,GH3030,GH3039,GH3128,GH4180,GH3044
Monel: Monel 400/K500/R405
Nitronic: Nitronic 40/50/60
Nimonic: Nimonic 75/80A/90/A263
Specification Wire: 0.01-10mm
Strip: 0.05*5.0-5.0*250mm
Bar: φ4-50mm;Length 2000-5000mm
Pipe: φ6-273mm;δ1-30mm;Length 1000-8000mm
Sheet: δ 0.8-36mm;Width 650-2000mm;Length 800-4500mm
Standard GB,AISI,ASTM,DIN,EN,SUS,UNS etc
Inspection ISO,SGS,BV and so on.
Application High temperature components such as turbine blades, guide vanes, turbine disks,
high pressure compressor disks,machine manufacturing
and combustion chambers used in the manufacture of aviation, naval and industrial gas turbines

We can provide customized services according to customer requirements

There are five main types of superalloys: nickel, iron, cobalt, titanium, and niobium.

1. Nickel-Based Superalloys
2. Iron-Based Superalloys
3. Cobalt-Based Superalloys
4. Titanium-Based Superalloys
5. Niobium-Based Superalloys

Superalloys are used in high-performance applications in which their enhanced properties can be exploited, as long as it is cost-effective to use them.

1. Medical Devices
2. Automotive Industry
3. Power Generation
4. Oil and Gas Industry
5. Chemical Processing
6. Electronics Industry
7. Military and Defense Industry
8. Aerospace Industry

factory-changjin
factory-changjin

We also provide forging blanks and CNC precision machining services for our clients, covering industries such as energy, petrochemicals, steel, engineering machinery, plastics, prevention and control, hydraulics, healthcare, and food. Please feel free to send us drawings for inquiries.

large-forgings-cnc 随机图片

Metalworking Services

CNC Machining

Sheet Metal Fabrication

Metal Welding

Metal Cutting

Metal Bending

Metal Punching

Metal Forging

Metal Sheet Rolling

Tube and Plate Drilling

Heavy Forging Press Capacity

Heavy Forging Press Capacity

Our heavy-duty forging presses support open-die forging and deformation of large-section forgings, including discs, shafts, blocks, and custom components. This capability enables us to meet the demanding forming requirements of heavy industrial applications.

Heat Treatment Capability

Heat Treatment Capability

Heat treatment is a critical step in achieving the mechanical properties required for heavy-duty forgings. Our process capabilities meet the strength, toughness, and structural stability requirements for forged components used under demanding operating conditions.

Heavy Shaft Machining

Heavy Shaft Machining

We offer machining capabilities for large forged shafts and long cylindrical components, supporting both rough and finish machining. This capacity is suitable for stepped shafts, rotor shafts, rollers, and other heavy-duty forged shaft components.

Ring Forging Machining

Ring Forging Machining

Our machining facilities are capable of handling large ring-shaped forgings and circular parts that require precise turning, face machining, boring, and contour control. This capability is suitable for industrial ring blanks, heavy-duty circular parts, and machined ring forgings.

Cylindrical Forging Machining

Cylindrical Forging Machining

We offer machining solutions for heavy-duty cylindrical, hollow, and tubular forgings. This capability supports the machining of sleeves, cylinders, and other thick-walled forged components used in pressure vessels, rotating systems, and general industrial applications.

Inspection & Testing

Inspection & Testing

Quality control is integrated into our production process through the inspection and testing of forged and machined parts. Our capabilities help verify the dimensional accuracy, condition, and quality consistency of industrial forgings prior to delivery.

Packing & Delivery

Packing & Delivery

Finished forgings are properly protected and packaged to minimize the risk of damage during storage and transportation. Our packaging methods ensure the safe domestic delivery and export shipment of machined and high-value forged components.

forging steel CNC Processing CNC Processing

Products Videos